Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

1048 Frit

Alternate Names: 1048 Alkalifritte

Description: Alkaline frit

Oxide Analysis Formula Tolerance
CaO 1.07% 0.07
MgO 0.07% 0.01
K2O 7.87% 0.29
Na2O 11.19% 0.63
Al2O3 22.77% 0.78
B2O3 17.39% 0.88
SiO2 39.64% 2.32
Oxide Weight 351.07
Formula Weight 351.07

Notes

Was available in Norway, manufacturer unknown. Info from http://www.potters.org/subject70375.htm

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy