| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.00% | 0.08 | |
| MgO | 0.20% | 0.02 | |
| K2O | 1.30% | 0.06 | |
| Na2O | 2.80% | 0.21 | |
| TiO2 | 0.29% | 0.02 | |
| Al2O3 | 22.00% | 1.00 | |
| SiO2 | 71.40% | 5.51 | |
| Fe2O3 | 0.65% | 0.02 | |
| LOI | 0.30% | n/a | |
| Oxide Weight | 461.97 | ||
| Formula Weight | 463.36 | ||
| Materials |
RC10 Vitreous
|
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Bulk Density g/cc (Packed) | 1.4 |
|---|---|
| Hardness (Moh) | 7 |
| Ultimate Particle Size Distribution | >71 micron: 1.6% |
| Density (Specific Gravity) | 2.6 |
| pH for dry powder | 7-8 |