Alternate Names: SaltLick
Description: A dark buff PCE 27 clay.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| MgO | 0.50% | 0.05 | |
| K2O | 2.30% | 0.10 | |
| Na2O | 0.10% | 0.01 | |
| TiO2 | 1.50% | 0.08 | |
| Al2O3 | 25.40% | 1.00 | |
| SiO2 | 60.90% | 4.07 | |
| Fe2O3 | 1.60% | 0.04 | |
| LOI | 7.50% | n/a | |
| Oxide Weight | 371.46 | ||
| Formula Weight | 401.57 | ||
| Materials |
Goldart
A plastic buff burning clay, often used as a major ingredient in stoneware clay bodies. |
| Materials |
Roseville Clay
|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk