March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | No tracking! No ads! No paywall! |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 1.10% | 0.04 | |
| Na2O | 0.20% | 0.01 | |
| MgO | 0.40% | 0.03 | |
| CaO | 0.20% | 0.01 | |
| TiO2 | 1.80% | 0.08 | |
| Fe2O3 | 0.90% | 0.02 | |
| Al2O3 | 29.00% | 1.00 | |
| SiO2 | 55.60% | 3.25 | |
| LOI | 11.40% | n/a | |
| Oxide Weight | 313.74 | ||
| Formula Weight | 354.11 | ||
If you know more about this material please contact us.
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Pyrometric Cone Equivalent | 32 |
|---|