FC-1 Filler Clay

Notes

From Laguna Clays: A blend of clay to replace PV Clay where certain reactions effect deflocculation, scumming, and discoloration of product.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials PV Clay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy