Description: Unknown
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 46.60% | 2.15 | |
| Al2O3 | 36.80% | 1.00 | |
| K2O | 1.00% | 0.03 | |
| MgO | 0.40% | 0.03 | |
| CaO | 0.50% | 0.02 | |
| LOI | 14.70% | n/a | |
| Oxide Weight | 236.43 | ||
| Formula Weight | 277.17 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |