Description: Zirconium silicate
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZrO2 | 67.21% | 1.00 | |
| SiO2 | 32.79% | 1.00 | |
| Oxide Weight | 183.34 | ||
| Formula Weight | 183.34 | ||
Also known as Zircopax Plus or Ultrox (see link below for more information).
| Materials |
Zircopax Plus
|
| Materials |
Zircon
|
| Materials |
Ultrox
|
| Hazards |
Zirconium Compounds Toxicity
|