CF Kaolin

Oxide Analysis Formula Tolerance
CaO 0.05% -
K2O 1.70% 0.05
MgO 0.30% 0.02
Na2O 0.10% -
TiO2 0.06% -
Al2O3 37.50% 1.00
SiO2 47.50% 2.15
Fe2O3 0.80% 0.01
LOI 11.80%n/a
Oxide Weight 239.39
Formula Weight 271.41

Notes

Particle Size Distribution:
>53 microns: 0.30 max

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.