Yellow Banks #101

Alternate Names: Yelo Banks 101

Oxide Analysis Formula Tolerance
CaO 0.70% 0.08
K2O 2.60% 0.17
MgO 1.40% 0.22
Na2O 1.00% 0.10
TiO2 1.00% 0.08
Al2O3 16.40% 1.00
SiO2 66.00% 6.83
Fe2O3 6.00% 0.23
LOI 5.00%n/a
Oxide Weight 591.48
Formula Weight 622.61

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.