1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Treopax

Oxide Analysis Formula Tolerance
Na2O 0.55% 1.00
TiO2 0.51% 0.72
ZrO 93.07% 97.87
Al2O3 0.50% 0.55
SiO2 5.23% 9.81
Fe2O3 0.14% 0.10
Oxide Weight 11,272.73
Formula Weight 11,272.73

Notes

A zircon opacifier that was used in the 1940s, 1950s.