Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Please don't panic, I am overwhelmed by the unbelievable support I am getting. We just need to get them to relent on this demand and call off the lawyer (to at least permit commentary). There are lots of backup sites (many people have the API endpoints), don't start downloading or scraping again and overload the server.

Insight-live.com general operation is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

T-Material

Notes

A a very refractory white clay with a high molochite content made by Morgan Refractories. Cheshire, UK (also available from Potclays, Stoke-on-Trent). (They also make Triton Kaowool ceramic fibre). It is much copied by other clay makers. It is an excellent hand building clay and a useful addition to raku bodies.

T-material was used by Hans Coper.
Y-material is a cheaper version of the same.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy