| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.87% | 0.03 | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 0.08% | - | |
| Al2O3 | 37.65% | 1.00 | |
| SiO2 | 46.23% | 2.08 | |
| Fe2O3 | 0.87% | 0.01 | |
| LOI | 14.11% | n/a | |
| Oxide Weight | 232.72 | ||
| Formula Weight | 270.95 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |