June 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: Shefield Clay
Description: Iron-rich native glacial clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 3.20% | 0.28 | |
| K2O | 4.00% | 0.21 | |
| MgO | 3.50% | 0.42 | |
| Na2O | 1.20% | 0.09 | |
| TiO2 | 1.00% | 0.06 | |
| Al2O3 | 19.60% | 0.93 | |
| SiO2 | 51.02% | 4.13 | |
| Fe2O3 | 8.50% | 0.26 | |
| LOI | 8.00% | n/a | |
| Oxide Weight | 447.33 | ||
| Formula Weight | 486.23 | ||
A native glacial iron-rich clay containing biotite, hornblende, chlorite, quartz, and other high Fe/Mg minerals. Sheffield Slip clay is based on this material.
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Materials |
Sheffield Slip
|