| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Se | 100.00% | 1.00 | |
| Oxide Weight | 111.20 | ||
| Formula Weight | 111.20 | ||
A metal of the sulfur group. It is normally added in its pure form to glass batches as a coloring agent for rose or ruby glass or to act as a decolorizer against green iron.
Selenium is also introduced from sodium selenite (Na2O SeO2) or barium selenite (BaO SeO2).
| Hazards |
Zirconium Encapsulated Stains Toxicity
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Hardness (Moh) | 4.5 |
|---|---|
| Frit Softening Point | 217C |