| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.45% | 0.04 | |
| Na2O | 0.45% | 0.05 | |
| TiO2 | 0.40% | 0.04 | |
| Al2O3 | 13.50% | 1.00 | |
| SiO2 | 79.00% | 9.93 | |
| Fe2O3 | 1.00% | 0.05 | |
| Cl | 5.20% | n/a | |
| Oxide Weight | 716.27 | ||
| Formula Weight | 755.56 | ||
Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.
| Materials |
Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings. |
| Materials |
Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc. |
| Materials |
Alkatrol
|
| Materials |
Pyrofrac
|
| Materials |
Seriphyl
|
| Bulk Density lbs/cu. ft. (Packed) | 65 |
|---|---|
| Pyrometric Cone Equivalent | 20 |
| Sieve Analysis Dry | +50 mesh: 0.1 +70 mesh: 0.1 +100 mesh: 1.1 +200 mesh: 8.6 +325 mesh: 21.0 |
| Density (Specific Gravity) | 2.6 |