| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.45% | 0.03 | |
| Na2O | 0.45% | 0.05 | |
| TiO2 | 0.40% | 0.04 | |
| Al2O3 | 14.50% | 1.00 | |
| SiO2 | 77.30% | 9.05 | |
| Fe2O3 | 1.00% | 0.04 | |
| H2O | 5.90% | n/a | |
| Oxide Weight | 661.94 | ||
| Formula Weight | 703.45 | ||
Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.
| Materials |
Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings. |
| Materials |
Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc. |
| Materials |
Alkatrol
|
| Materials |
Pyrofrac
|
| Bulk Density lbs/cu. ft. (Packed) | 100 |
|---|---|
| Pyrometric Cone Equivalent | 20 |
| Sieve Analysis Dry | +20 mesh: 0.1 +50 mesh: 12.0 +70 mesh: 16.0 +100 mesh: 20.0 +200 mesh: 26.5 +325 mesh: 14.0 |
| Density (Specific Gravity) | 2.6 |