Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

1D Sandy Stoneware

Description: PR#1 D, Buff Burning Sandy Stoneware

Oxide Analysis Formula Tolerance
CaO 0.13% 0.02
K2O 2.64% 0.19
MgO 0.38% 0.07
Na2O 0.16% 0.02
TiO2 0.60% 0.05
Al2O3 14.66% 1.00
P2O5 0.02% -
SiO2 75.38% 8.73
Fe2O3 1.02% 0.04
MnO 0.01% -
LOI 5.67%n/a
Oxide Weight 660.98
Formula Weight 700.71

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy