| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 48.50% | 1.00 | |
| Cr2O3 | 51.50% | 0.66 | |
| Oxide Weight | 194.23 | ||
| Formula Weight | 194.23 | ||
A soluble crystalline bright yellow powder. It is used to introduce Chromium oxide into low temperature glazes to achieve colors such as red. The chromium is more effectively dispersed because it is combined with potassium.
| Materials |
Potassium Dichromate
|
| Hazards |
Chromium Compounds Toxicology
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |