Description: A bright red-orange crystalline powder
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 32.02% | 1.00 | |
| Cr2O3 | 67.98% | 1.32 | |
| Oxide Weight | 294.19 | ||
| Formula Weight | 294.19 | ||
| Materials |
Potassium Chromate
|
| Hazards |
Chromium Compounds Toxicology
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| URLs |
http://en.wikipedia.org/wiki/Potassium_dichromate
Potassium Dichromate at Wikipedia |
| URLs |
http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc13/icsc1371.htm
Potassium Dichromate at ilo.og |
| Oxides | Cr2O3 - Chrome Oxide |