Description: FLINT
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 0.35% | 1.00 | |
| SiO2 | 99.40% | 482.00 | |
| Fe2O3 | 0.04% | 0.07 | |
| LOI | 0.18% | n/a | |
| Oxide Weight | 29,081.66 | ||
| Formula Weight | 29,134.10 | ||
Sieve Analysis:
% Thru: 100# 200 325 mesh
===========================
#120 Flour 88.0 64.0 44.0
#180 Flour 98.8 96.0 77.0
#200 99.9 98.0 85.0
#325 99.9 99.8 96.6
#375 99.9 99.8 98.0
Many grades and sizes of sand also available.
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |