Description: 30 mesh silica
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 98.00% | 1.00 | |
| LOI | 0.50% | n/a | |
| Oxide Weight | 60.10 | ||
| Formula Weight | 60.40 | ||
| Materials |
Silica Sand
|
| Temperatures | Quartz inversion (alpha-beta) (540-600) |
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |