1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Zinc Oxide-Alumina-Silicate Eutectic

Oxide Analysis Formula Tolerance
ZnO 51.30% 1.00
Al2O3 14.50% 0.23
SiO2 34.20% 0.90
Oxide Weight 158.67
Formula Weight 158.67

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1360C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen