Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server may not be operational under later tommorrow. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Zinc and Cadmium Metasilicate Eutectic

Formula: ZnSiO3 . 1.75CdSiO3

Oxide Analysis Formula Tolerance
ZnO 17.20% 0.36
CdO 47.60% 0.64
SiO2 35.20% 1.01
Oxide Weight 171.82
Formula Weight 171.82

Related Information

Links

Glossary Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures.
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1052C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy