Oxide Analysis Formula Tolerance
B2O3 0.10% -
CaO 8.54% 0.32
MgO 4.02% 0.21
Na2O 13.55% 0.46
K2O 0.10% -
Al2O3 0.50% 0.01
SiO2 72.79% 2.57
Fe2O3 0.10% -
SO3 0.30%n/a
Oxide Weight 211.41