Float Glass

Description: Typical float glass

Oxide Analysis Formula Tolerance
CaO 8.80% 0.33
MgO 3.80% 0.20
Na2O 13.80% 0.47
SiO2 73.50% 2.58
Al2O3 0.20% -
Oxide Weight 211.30
Formula Weight 211.30

Related Information

Links

URLs http://www.glassproperties.com/glasses/
Glassproperties.com
Materials Container Glass
Materials Glass Cullet
Materials Window Glass

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy