| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 66.00% | 7.05 | 0.5 |
| Al2O3 | 17.70% | 1.11 | 0.5 |
| Fe2O3 | 0.10% | - | Max |
| K2O | 11.00% | 0.75 | Min |
| Na2O | 2.10% | 0.22 | 0.75 |
| CaO | 0.25% | 0.03 | |
| MgO | 0.03% | - | |
| LOI | 0.30% | n/a | |
| Oxide Weight | 623.57 | ||
| Formula Weight | 625.45 | ||
Intended for ceramics and glass.
K2O in minimum figure.
Fe2O3 is maximum figure.
LOI is maximum figure.
Available in 1200, 1250 and 1350 bulk bags and 25, 40 and 50 bags.
Available in 100, 200, 325 mesh sizes.

This picture has its own page with more detail, click here to see it.
From India, Imerys Ceramics