Strontium Aluminum Silicate Eutectic

Oxide Analysis Formula Tolerance
SrO 53.70% 1.00
Al2O3 21.20% 0.40
SiO2 25.10% 0.81
Oxide Weight 192.92
Formula Weight 192.92

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1290C

PayPal