Stains (inclusion)

Notes

These pigments give color stability at stoneware temperatures in reduction and oxidation. Cadmium and Selenium particles are combined with Zirconium to stabilize them against dissolution into the melt. Reds and orange hues which are very difficult to achieve in reduction are now possible. These stains are very expensive and must be used according to instructions.

Related Information

How to include stains in chemistry calculations in Insight


This picture has its own page with more detail, click here to see it.

The simple answer is that you should not. The chemistry of stains is proprietary. Stain particles do not dissolve into the glaze melt like other materials, they suspend in the transparent glass to color it. That is why stains are color stable and dependable. In addition, their percentage in the recipe, not the formula, is the predictor of their effect on the fired glaze. Of course they do impose effects on the thermal expansion, melt fluidity, etc., but these must be rationalized by experience and testing. But you can still enter stains into Insight recipes. Consider adding the stains you use to your private materials database (for costing purposes for example).

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy