Description: Vanadium Greens (ZrPrV, ZrVSn, ZrV)
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Stain
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Body Color | Admirably suited to staining all types of bodies because of freedom from tendency to strike or flash. In reducing conditions, tin-based greens should not be used. |
|---|---|
| Glaze Color | Suitable for all types of glazes for firing at temperatures up to over 1300C (1250C for Zr-Pr-V). Zircon is recommended as an opacifier, although tin oxide may also be used. Underglaze Color: Suitable for all methods of underglaze decoration. Unlike victoria greens, vanadium greens are suitable for use under all types of glazes. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk