June 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Ag2O | 83.04% | 1.00 | |
| PO4 | 22.69% | 0.67 | |
| Oxide Weight | 295.05 | ||
| Formula Weight | 295.05 | ||