Description: Cuban silica
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 0.10% | 0.16 | |
| MgO | 0.06% | 0.25 | |
| CaO | 0.25% | 0.75 | |
| SiO2 | 99.16% | 277.52 | |
| Fe2O3 | 0.02% | 0.02 | |
| LOI | 0.18% | n/a | |
| Oxide Weight | 16,751.44 | ||
| Formula Weight | 16,781.64 | ||
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
| Materials |
Silica Teresa (Cuba)
|
| Materials |
Silica D/Golpe (Cuba)
|
| Materials |
Silica Santa Barbara (Cuba)
|
| Materials |
Silica De Mármol (Cuba)
|
| Materials |
Silica Arimao (Cuba)
|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk