Silica De Mármol (Cuba)

Description: Cuban silica

Oxide Analysis Formula Tolerance
Al2O3 1.03% 0.49
MgO 0.30% 0.36
CaO 0.75% 0.64
SiO2 97.00% 77.55
Fe2O3 0.70% 0.21
0.23% -
LOI 0.48%n/a
Oxide Weight 4,794.08
Formula Weight 4,817.21

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
Materials Silica Sierra Cristal (Cuba)