Sandblend 90sl Ball

Description: SLURRIED REFINED DEVON BALLCLAY

Oxide Analysis Formula Tolerance
CaO 0.20% 0.01
K2O 2.20% 0.09
MgO 0.03% -
Na2O 0.40% 0.02
TiO2 1.30% 0.06
Al2O3 27.90% 1.00
SiO2 56.50% 3.44
Fe2O3 1.00% 0.02
LOI 10.20%n/a
C 1.80%n/a
Oxide Weight 327.31
Formula Weight 371.95

Notes

Particle Size (e.s.d.)
125 microns - <.05
10 microns - 95
2 microns - 76
1 microns - 65
Modulus of Rupture at 110C
Mn/M2 - 7.3
lbf/in2 - 1050
Water Absorption
1120C - 1.0
1220C - 0.50
Shrinkage Dry to Fired
1120C - 11.00
1220C - 12.00
Reflectance 464nm
1120C - 75
1220C - 53
Refractoriness
Cone - 32, 1710C

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy