Pyrophyllite PPRG53

Oxide Analysis Formula Tolerance
K2O 1.00% 0.07
Na2O 0.10% 0.01
TiO2 0.20% 0.02
Al2O3 15.80% 1.00
SiO2 79.40% 8.53
Fe2O3 0.40% 0.02
LOI 3.10%n/a
Oxide Weight 625.56
Formula Weight 645.57

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy