PotteryCrafts Frit P2957

Alternate Names: PotteryCrafts Frit 2957

Description: Low expansion borax frit

Oxide Analysis Formula Tolerance
CaO 7.30% 0.59
MgO 0.20% 0.02
K2O 2.70% 0.13
Na2O 3.60% 0.26
Al2O3 9.40% 0.42
B2O3 14.80% 0.96
SiO2 62.00% 4.65
Oxide Weight 450.83
Formula Weight 450.83

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 5.9
Frit Melting Range (C) 1000-1100C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy