Alternate Names: PotteryCrafts Frit 2955
Description: High alkali low alumina borax frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.80% | 0.37 | |
| K2O | 8.80% | 0.22 | |
| Na2O | 10.90% | 0.41 | |
| B2O3 | 13.50% | 0.46 | |
| Al2O3 | 9.10% | 0.21 | |
| SiO2 | 48.90% | 1.91 | |
| Oxide Weight | 234.69 | ||
| Formula Weight | 234.69 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Frit J
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information |
| Co-efficient of Linear Expansion | 10.9 |
|---|---|
| Frit Melting Range (C) | 920-1050C |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk