Polyvinyl Alcohol

Notes

Used as a binder in ceramic bodies.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Additives for Ceramic Bodies
Materials that are added to bodies to impart physical working properties and usually burn away during firing. Binders enable bodies with very low or zero clay content to have plasticity and dry hardness, they can give powders flow properties during pressing and impart rheological properties to clay slurries. Among potters however, it is common for bodies to have zero additives.
URLs http://en.wikipedia.org/wiki/Polyvinyl_alcohol
Polyvinyl Alcohol at Wikipedia
Articles Binders for Ceramic Bodies
An overview of the major types of organic and inorganic binders used in various different ceramic industries.
Materials Methylcellulose

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy