Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-63

Alternate Names: Frit Pb63

Description: Medium lead frit

Oxide Analysis Formula Tolerance
CaO 4.50% 0.29
Na2O 3.60% 0.21
PbO 30.50% 0.50
ZrO2 2.40% 0.07
B2O3 12.60% 0.66
Al2O3 3.40% 0.12
SiO2 43.00% 2.60
Oxide Weight 363.73
Formula Weight 363.73

Related Information

Links

Materials Pemco Frit Pb-742
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3417
Materials Hommel Frit 24
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.8 x 10-6 (50-450C)
Frit Melting Range (C) 1350-1460F
I.F.P. (celsius) 565C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy