Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
Alternate Names: Frit P-316, Pemco 316, Pemco Frit Pb316
Description: Lead-alumina-sillicate eutectic
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 61.30% | 1.00 | |
| Al2O3 | 7.00% | 0.25 | |
| SiO2 | 31.69% | 1.92 | |
| Oxide Weight | 364.07 | ||
| Formula Weight | 364.07 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 4GF79D
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.0 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1400-1550F |
| I.F.P. (celsius) | 635C |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk