Pemco Frit Pb-1421

Alternate Names: Frit Pb1421

Description: Leaded low borax frit

Oxide Analysis Formula Tolerance
CaO 8.30% 0.50
K2O 1.80% 0.06
Na2O 2.70% 0.15
PbO 19.30% 0.29
B2O3 6.00% 0.29
Al2O3 6.50% 0.21
SiO2 55.40% 3.10
Oxide Weight 336.61
Formula Weight 336.61

Notes

Frit for all-fritted base firing in the range of Cone 05 through Cone 6. This glaze is somewhat similar to a blend of Pb-349 and Pb-742

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.6 x 10-6 (50-450C)
Frit Softening Point 1550F
Frit Melting Range (C) 1500-1650F
I.F.P. (celsius) 610C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy