Alternate Names: 4N57,4N-57
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Li2O | 0.30% | 0.08 | |
| Na2O | 6.84% | 0.92 | |
| B2O3 | 18.84% | 2.25 | |
| Al2O3 | 7.16% | 0.58 | |
| SiO2 | 66.87% | 9.25 | |
| Oxide Weight | 831.08 | ||
| Formula Weight | 831.08 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |