Pemco Frit P-404

Alternate Names: Frit 404, Frit P404

Description: High temperature leadless boron free glaze flux

Oxide Analysis Formula Tolerance
BaO 17.80% 0.22
CaO 12.20% 0.41
K2O 12.00% 0.24
Na2O 4.60% 0.14
Al2O3 10.80% 0.20
SiO2 42.60% 1.32
Oxide Weight 186.86
Formula Weight 186.86

Related Information

Links

Materials Ferro Frit 3831
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 488
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 13.00
Co-efficient of Linear Expansion 13.0 x 10-6 (50-450C)
Frit Melting Range (C) 1430-1960F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy