Hommel Frit 488

Oxide Analysis Formula Tolerance
K2O 12.01% 0.24
Na2O 4.59% 0.14
CaO 12.16% 0.41
BaO 17.81% 0.22
Al2O3 10.83% 0.20
SiO2 42.60% 1.33
Oxide Weight 187.10
Formula Weight 187.10

Related Information

Links

Materials Pemco Frit P-404
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 11.7 x 10-6
Frit Melting Range (C) 1580F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy