Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-238

Alternate Names: Frit 238, Frit P238

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
K2O 3.10% 0.22
Na2O 7.20% 0.78
B2O3 31.70% 3.06
Al2O3 16.50% 1.09
SiO2 41.50% 4.63
Oxide Weight 670.97
Formula Weight 670.97

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 579
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.6 x 10-6 (50-450C)
Co-efficient of Linear Expansion 7.6 x 10-6 (50-450C)
Frit Melting Range (C) 1450-1560F
I.F.P. (celsius) 535C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy