Description: Super-white ball clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 50.60% | 2.51 | |
| Al2O3 | 34.20% | 1.00 | |
| Fe2O3 | 0.72% | 0.01 | |
| TiO2 | 0.43% | 0.02 | |
| CaO | 0.06% | - | |
| MgO | 0.08% | 0.01 | |
| K2O | 1.26% | 0.04 | |
| Na2O | 0.11% | 0.01 | |
| LOI | 12.54% | n/a | |
| Oxide Weight | 260.85 | ||
| Formula Weight | 298.25 | ||
Excellent plasticity and reasonable particle distribution and it can improve the speed and quality when making semi-finished ceramic products. Application in high-grade polished tiles, porcelain tiles, sanitary ware,etc .
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |
| URLs |
http://www.opeal.com.cn/english/products_op03.htm
OP-3 Ball Clay information |