Mulcoa 60 Calcine Grog

Description: Mullite grog

Oxide Analysis Formula Tolerance
Al2O3 58.60% 1.00
SiO2 37.80% 1.09
TiO2 2.20% 0.05
Fe2O3 1.13% 0.01
Oxide Weight 173.59
Formula Weight 173.59

Notes

Other grades are available, see them for more information.

Related Information

Links

Materials Grog
Materials Mulcoa 70 Mullite
Materials Mulcoa 47 Calcine Grog
Typecodes Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes.

Data

Pyrometric Cone Equivalent 37

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy