Description: Mullite grog
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 46.80% | 1.00 | |
| SiO2 | 50.00% | 1.81 | |
| TiO2 | 1.90% | 0.05 | |
| Fe2O3 | 0.95% | 0.01 | |
| Oxide Weight | 217.19 | ||
| Formula Weight | 217.19 | ||
A number of grades are available and are used in the refractory industry.
| Materials |
Grog
|
| Materials |
Mulcoa 60 Calcine Grog
|
| Materials |
Mulcoa 70 Mullite
|
| Typecodes |
Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes. |