Description: Fritte boro-calcique
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 38.40% | 1.00 | |
| B2O3 | 47.70% | 1.00 | |
| Al2O3 | 7.70% | 0.11 | |
| SiO2 | 6.20% | 0.15 | |
| Oxide Weight | 146.09 | ||
| Formula Weight | 146.09 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 660C |
|---|