Moulin Fritte M85

Description: Fritte boro-alcaline

Oxide Analysis Formula Tolerance
B2O3 37.00% 4.71
Na2O 7.00% 1.00
SiO2 56.00% 8.25
Oxide Weight 885.71
Formula Weight 885.71

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 505C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy