Description: Fritte plombo-boracique
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 62.30% | 1.00 | |
| B2O3 | 29.30% | 1.51 | |
| SiO2 | 8.40% | 0.50 | |
| Oxide Weight | 358.27 | ||
| Formula Weight | 358.27 | ||
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 495C |
|---|